Specifications and Mixing Ratio
| D.R.BOND 2460 | DRODUR 75 |
| Solids Content | 60 +/- 2% | 75 +/- 2% |
| Carrier Solvent | Ethyl Acetate | Ethyl Acetate |
| Color | Colorless to pale yellow | Colorless to pale yellow |
| Appearance | Transparent | Transparent |
| Odor (After drying) | Odorless | Odorless |
| Mix. Ratio | 100 parts by weight | 10 parts by weight |
Viscosity Profile
| Solids Content | 25% | 30% | 35% |
| D.R. BOND 2460 (Kg) | 1 | 1 | 1 |
| DRODUR 75 (Kg) | 0.1 | 0.1 | 0.1 |
| Ethyl Acetate (Kg) | 1.54 | 1.09 | 0.774 |
| Viscosity in seconds | 15 – 18 | 18.5 –23.0 | 23.5 –30.5 |
| (By B-4 ford cup @ 30°C | | | |
Performance Characteristics: The bond strength immediately after lamination is good. The laminates can be subjected to secondary operations like second ply lamination, rewinding, slitting etc. after 10 hours of initial lamination, provided all the process control parameters are adhered to while lamination and the laminate quality is good. The adhesive system will require at least 8 days to develop its optimum heat and chemical resistant properties.