IndiaMART.com

Products & Services

Acid Proof Material

We offer a broad assotment of acid proof bricks as well as mortars. Acid proof bricks are manfactured with high quality materials, and the manufacturing process is supervised by our expert team of quality controllers.

Acid Resistant Cement

Acid Resistant Cement

 

We trade and supply Acid Resistant Cements for our clients that find wide application in various manufacturing units. Various types of chemicals are used extensively as penetrating concrete sealers. The silica reacts with free calcium in the concrete and forms calcium silicate hydrate that results in a concrete surface. These are widely appreciated for their features like abrasion-resistant, chemically resistant, hardness and less permeability. Potassium silicate can be used to prevent whitish blooming or efflorescence because oil well cements are relatively high in water content, meta silicates are added to help prevent segregation of the solids from the water. The wide range of acid resistant cements we export are made up of these chemicals.

 

ARI-AR 2 Acid Proof Material

Bricks & Tiles :ARI-AR(230*115*38MM)

 

Physical Properties -

Water Absorption (%) :2.0

Cold Crushing Strength(N/mm2) :70

Flexure Strength(N/mm2) :10

Acid Resistance(%loss in weight) :2.5

 

Chemical Properties -

SiO3(%) :68.20

Al2O3(%) :24.00

Fe2O3(%) :1.8

TiO2(%) : 2.10

CaO+MgO(%) :0.50

Na2O+K2O(%) :3.40

Weight of Brick(Kg) :4.35

Application Properties :For Acid Storage Tank,Floor & Acid Designer.

 

Mortars :Sodium silicate base mortar

Working Time(min at 270+20C) (minutes) :15

Flexure Strength (min kg/cm2)(at 7 days) :35

Compressive Strength(Min. Kg/cm2)(at 7 days ):100

Bond strength(Min. Kg/cm2) :5

Absorption of Tolerance(Max % by weight) :18

Application Area :For laying of Acid Resistant Brick &Tiles.

 

 

Mortars :Potassium silicate base mortar

Working Time(min at 270+20C) (minutes) :20

Flexure Strength (min kg/cm2)(at 7 days) :40

Compressive Strength(Min. Kg/cm2)(at 7 days ):150

Bond strength(Min. Kg/cm2) :5

Absorption of Tolerance(Max % by weight) :18

Application Area :For laying of Acid Resistant Brick &Tiles.

 

ARI-AR 1 Acid Proof Material

Bricks &Tiles :ARI-AR(230*100*20MM)

 

Physical Properties -

Water Absorption (%) :2.0

Cold Crushing Strength(N/mm2) :70

Flexure Strength(N/mm2) :20

Acid Resistance(%loss in weight) :1.5

 

Chemical Properties -

SiO3(%) :67.90

Al2O3(%) :24.20

Fe2O3(%) :1.9

TiO2(%) : 2.90

CaO+MgO(%) :0.60

Na2O+K2O(%) :3.60

Weight of Brick(Kg) :0.90

Application Properties :For Battery Room,Acid Handling Floor &DM Floor.

 

Mortars :Sodium silicate base mortar

Working Time(min at 270+20C) (minutes) :15

Flexure Strength (min kg/cm2)(at 7 days) :35

Compressive Strength(Min. Kg/cm2)(at 7 days ):100

Bond strength(Min. Kg/cm2) :5

Absorption of Tolerance(Max % by weight) :18

Application Area :For laying of Acid Resistant Brick &Tiles.

 

 

Mortars :Potassium silicate base mortar

Working Time(min at 270+20C) (minutes) :20

Flexure Strength (min kg/cm2)(at 7 days) :40

Compressive Strength(Min. Kg/cm2)(at 7 days ):150

Bond strength(Min. Kg/cm2) :5

Absorption of Tolerance(Max % by weight) :18

Application Area :For laying of Acid Resistant Brick &Tiles.

 

ARI-AR 3 Acid Proof Material

Bricks &Tiles :ARI-AR(230*115*75MM)

 

Physical Properties -

Water Absorption (%) :2.0

Cold Crushing Strength(N/mm2) :70

Flexure Strength(N/mm2) :10

Acid Resistance(%loss in weight) :2.5

 

Chemical Properties -

SiO3(%) :68.20

Al2O3(%) :24.00

Fe2O3(%) :1.8

TiO2(%) : 2.10

CaO+MgO(%) :0.50

Na2O+K2O(%) :3.40

Weight of Brick(Kg) :4.35

Application Properties :For Thermal Power Plant Chimney&Acid Storage

Tank & Floor.

 

Mortars :Sodium silicate base mortar

Working Time(min at 270+20C) (minutes) :15

Flexure Strength (min kg/cm2)(at 7 days) :35

Compressive Strength(Min. Kg/cm2)(at 7 days ):100

Bond strength(Min. Kg/cm2) :5

Absorption of Tolerance(Max % by weight) :18

Application Area :For laying of Acid Resistant Brick &Tiles.

 

 

Mortars :Potassium silicate base mortar

Working Time(min at 270+20C) (minutes) :20

Flexure Strength (min kg/cm2)(at 7 days) :40

Compressive Strength(Min. Kg/cm2)(at 7 days ):150

Bond strength(Min. Kg/cm2) :5

Absorption of Tolerance(Max % by weight) :18

Application Area :For laying of Acid Resistant Brick &Tiles.

 

To,Monolithic Sales Corporation

Promote Your Business with IndiaMART
Enter Your Website URL
RELATED COMPANIES