Epoxy Polyester Powder We produce premium grade epoxy polyester powder. Our epoxy polyester powder are used in general purposes like interior use for decoration and industrial application.
Technical details of our epoxy polyester powder are:
| Curing Schedule | 190°C/ 10 min. (Metal Temperature). | | Shade | As per customer requirement. | | Finish | Glossy, Semi-glossy,Matt Textured/ Structure as per customer requirement. | | Pack Size | 10kg/ 20kg. | | Shelf Life | 6 months from the date of manufacture if stored in a cool dry place. | | Recommended DFT | 50-55 Micron | | Flexibility | Passes 3.0 to 6.0mm by conical mandrel. | | Adhesion (2mm) | GT=0 | | Gloss @ 60° | As per customer requirement. | | Scratch Hardness | Above 4.0 kg | | Erichsen Cupping | Minimum 7.0 kg | | Impact Resistance | Minimum 80kg/cm (5/8'' ball dia) | | Salt Spray Resistance | Passes 1000 hrs. | | Humidity Resistance | Passes 1000 hrs. | | Covering Capacity | For smooth finish 110 sq.ft./ kg when applied at 50-55 micronassuming 95.0% utilization. |
| |
|
Fusion Bonded Epoxy Powder We manufacture an excellent grade fusion bonded epoxy powder. Effective in providing superior quality coatings and suitable for applications on exterior / Interior of D.I./ C.I. and steel pipes / fittings.
Technical Features:
| Curing Schedule | Fusion bonding at 3'/220°C. | | Shade | As per customer requirement. | | Finish | Glossy, Semi-glossy | | Pack Size | 10kg/ 20kg. | | Shelf Life | 6 months from the date of manufacture if stored below 30°C in a dry place | | Recommended DFT | 300-350 Micron | | Test Substrate | 0.8mm thick steel sand blasted | | Curing | 10 min at 200°C | | Application DFT | 60-70 Micron | | Erichsen Cupping | Passes 8.0mm | | Impact Resistance | Passes 160 sq. mm. | | Salt Spray Resistance | Passes 1000 hrs. | | Humidity Resistance | Passes 1000 hrs. | | Boiling Water Test (10 Days) | No Blistering | | Covering Capacity | 110-120 sq.ft./ kg when applied at 50-55 micron assuming 95.0%utilization |
| |
|
Metallic Powder We manufacturer metallic powder of superior quality. This powder is used in painting of wheel Rim and in various applications.
| |
|
Pure Epoxy Powder We manufacture pure epoxy powder of superior quality. Our epoxy powder range is recommended for products exposed to most punishing atmosphere. We also offer insulation grade epoxy powder.
Technical Features:
| Curing Schedule | 190°C/ 10 min. (Metal Temperature). | | Shade | As per customer requirement. | | Finish | Glossy, Semi-glossy and Matt and Text/ Structure as per customerrequirement. | | Pack Size | 10kg/ 20kg. | | Shelf Life | 6 months from the date of manufacture if stored in a cool dryplace. | | Recommended DFT | 50-55 Micron | | Flexibility | Passes 3.0 to 6.0mm by conical mandrel. | | Adhesion (2mm) | GT=0 | | Gloss @ 60° | As per customer requirement. | | Scratch Hardness | Above 4.0 kg | | Erichsen Cupping | Minimum 4.0 kg | | Impact Resistance | Minimum 80kg/cm (5/8'' ball dia) | | Salt Spray Resistance | Passes 1000 hrs. | | Humidity Resistance | Passes 1000 hrs. | | Covering Capacity | For smooth finish 110 sq.ft./ kg when applied at 50-55 micronassuming 95.0% utilization. |
| |
|
Pure Polyester Powder We manufacture pure polyester powder that are most suited for outdoor applications where excellent weatherability is required.
Technical specifications:
| Curing Schedule | 190°C/ 10 min. (Metal Temperature). | | Shade | As per customer requirement. | | Finish | Glossy, Semi-glossy, Matt Textured/ Structure as per customer requirement. | | Pack Size | 10kg/ 20kg. | | Shelf Life | 6 months from the date of manufacture if stored in a cool dry place. | | Recommended DFT | 50-55 Micron | | Flexibility | Passes 3.0 to 6.0mm by conical mandrel. | | Adhesion (2mm) | GT=0 | | Gloss @ 60° | As per customer requirement. | | Scratch Hardness | Above 4.0 kg | | Erichsen Cupping | Minimum 7.0 kg | | Impact Resistance | Minimum 80kg/cm (5/8'' ball dia) | | Salt Spray Resistance | Passes 1000 hrs. | | Humidity Resistance | Passes 1000 hrs. | | Covering Capacity | For smooth finish 110 sq.ft./ kg when applied at 50-55 micron assuming 95.0% utilization. |
| |
|