SP 509 Bronze Master Alloys
Ask For Price

SP 509 Bronze Master Alloys

Get Price

Melting Temp of Alloy : 940 0C

Application: The alloy SP 509 is a ready to use alloy for imitation and fashion jewellery, imparting a pleasant yellow color. It is an all-purpose alloy, usable for both hand-made, investment cast and spin cast jewellery, and is suitable for gold and silver plating.

Recommended Practice:

Application : Casting / H-made

Casting Temp. : 10500C - 10800C

Flask Temp. [Normal Cast] : 6300C - 6500C

Flask Temp. [Stone Cast] : 5900C – 6200C

Quenching Time : 25 - 30 minutes

Notes:
The actual casting temperatures and flask temperatures shall be decided by the parameters like the section thickness of the items (thick, medium or thin), the overall size/bulk of the cast tree, the design intricacies etc.
As a thumb rule, for thinner sections higher temperatures are selected and for thicker sections lower temperatures are preferred. At the same time, designs demanding higher form filling capabilities, higher than normal temperatures are an obvious choice.
Cast Tree Cleaning & Drying procedure: After primary removal of the investment during quenching, submerge tree in a hot (80-100oC) 50% phosphoric acid solution for 15-20 minutes. Rinse well with cool water to remove remaining investment powder and base metal oxides. Dry with compressed air.

Yes! I am interested

Request Callback
SP 505 Yellow Brass Master Alloys
Ask For Price

SP 505 Yellow Brass Master Alloys

Get Price

Melting Temp of Alloy : 910 0C

Application: The alloy SP 505 is a ready to use alloy for imitation and fashion jewellery, imparting a pleasant yellow color. It is an all-purpose alloy, usable for both hand-made; investment cast and spin cast jewellery, and is suitable for gold and silver plating.

Recommended Practice:

Application : Casting / H-made

Casting Temp. : 10300C - 10500C

Flask Temp. [Normal Cast] : 6200C - 6400C

Flask Temp. [Stone Cast] : 5800C – 6000C

Quenching Time : 15 - 20 minutes

Notes:
The actual casting temperatures and flask temperatures shall be decided by the parameters like the section thickness of the items (thick, medium or thin), the overall size/bulk of the cast tree, the design intricacies etc.
As a thumb rule, for thinner sections higher temperatures are selected and for thicker sections lower temperatures are preferred. At the same time, designs demanding higher form filling capabilities, higher than normal temperatures are an obvious choice.
Cast Tree Cleaning & Drying procedure: After primary removal of the investment during quenching, submerge tree in a hot (80-100oC) 50% phosphoric acid solution for 15-20 minutes. Rinse well with cool water to remove remaining investment powder and base metal oxides. Dry with compressed air.

Yes! I am interested

Request Callback

SP 507 Yellow Brass Master Alloys For Imitation and Cad Work

SP 507 Yellow Brass Master Alloys For Imitation and Cad Work

Ask For Price

Reach Us

Gmap

Mehta Distributors A-11, Zaveri Chambers, Behind Golden, Soni Bazar, Behind Golden, Soni Bazar,
Rajkot-360001, Gujarat, India

Munjal Mehta ( Proprietor )
08046083613Call Response Rate: 77%
Send SMS
Send E-MAIL

Share Us:


We are here to Help You!
Go Mobile : Follow Us On :
Copyright © 1996-2018 IndiaMART InterMESH Ltd. All rights reserved.